Architectural
Specifications - WMP-VR-R PLUS
|
ENGLISH |
|
Fiberglass shall be as outlined in the North American
Insulation Manufacturing Association (NAIMA 202-96) specification,
or equal, with an R-value of ______ when not compressed. The
fiberglass shall be faced with ______, as specified below, on one
side. The composite of fiberglass and facing shall have
surface burning characteristics not to exceed 25 flame spread and 50
smoke developed when tested in accordance with Underwriters
Laboratories 723 test method or ASTM E 84 test method.
Facing shall be composed of 0.0015” white polypropylene film, a reinforcing
layer, and 0.0005” metallized polyester film. The product shall be reinforced
with a 4x4 tri-directional fiberglass scrim. The resulting facing shall have a
water vapor transmission rate of 0.02 US perm (ASTM E96, Procedure A), and a
mullen burst of 100 P.S.I. Tensile strength shall be 35# in the machine
direction and 35# in the cross-machine direction.
|
|
METRIC |
|
Fiberglass shall be as outlined in the North American
Insulation Manufacturing Association (formerly T.I.M.A )
specification, or P.E.B. 202 or equal, with an R-value of ______
when not compressed. The fiberglass shall be faced on one
side. The composite of fiberglass and facing shall have
surface burning characteristics not to exceed 25 flame spread and 50
smoke developed when tested in accordance with Underwriters
Laboratories 723 test method or ASTM E 84 test method.
Facing shall be composed of 38.1 micron white polypropylene film, a reinforcing
layer, and 12.7 micron metallized polyester film. The product shall be
reinforced with a 16/100 mm x 16/100 mm tri-directional fiberglass scrim. The
resulting facing shall have a water vapor transmission rate of 1.15 ng/N.s
(ASTM E96, Procedure A), and a mullen burst of 7.0 kg/cm². Tensile strength
shall be 6.1 kN/m in the machine direction and 6.1 kN/m in the cross-machine
direction.
|
|