Product Specification: WMP-ASJ

POLYPROPYLENE / CORE / SCRIM / FOIL

 

Meets ASTM C1136, Type I, II, III, IV
(click for PDF format)

 

FACING COMPOSITION DESCRIPTION VALUES (ENGLISH) VALUES (METRIC)
White Film Polypropylene 0.0015 inch 38.1 micron
Adhesive Flame Resistant    
Core Proprietary 38 lbs / 300 ft² 62 gm / m²
Adhesive Fire Retardant    
Reinforcing Tri-directional
Fiberglass
5 / inch (MD) 5 / inch (XD) 20 / 100 mm (MD)
20 / 100 mm (XD)
Barrier Coating Polymeric    
Foil Aluminum 0.0003 inch 7.6 micron

 

PHYSICAL PROPERTIES TEST METHOD VALUES (ENGLISH) VALUES (METRIC)
Basis Weight Scale 34 lbs / 1000 ft² 166 gm / m²
Permeance (WVTR) ASTM E96 Procedure A 0.02 perm (grains/hr.ft².in Hg) 1.15 ng / N.s
Bursting Strength ASTM D774 120  psi 8.4 kg / cm²
Puncture Resistance ASTM C1136 60 beach units 1.8 Joules
Tensile Strength ASTM C1136 80 lbs/inch width (MD)
60 lbs/inch width (XD)
14.0 kn / m (MD)
10.5 kn / m (XD)
Caliper / Thickness Micrometer 0.009 inch 229 micron
Accelerated Aging 30 Days @ 95% RH,
120°F (49°C)
No Corrosion
No Delamination
No Corrosion
No Delamination
Low Temperature Resistance ASTM D1790 -40°F (-40°C) Remains Flexible No Delamination Remains Flexible No Delamination
High Temperature Resistance 4 hours @ 240°F (116°C) Remains Flexible No Delamination Remains Flexible No Delamination
Water Immersion 24 hours @ 73°F (23°C) No Delamination No Delamination
Mold Resistance ASTM C665 / C1338 No Growth No Growth
Dimensional Stability ASTM D1204 0.25% 0.25%

 

FIRE TESTING

ASTM E84

Polypropylene Side Exposed

Flame Spread

10

Smoke Developed

30

Physical Properties based upon statistical averages, Weight / Thickness +/- 10%